EN-GJSA-XNiCrNb20-2
Cast Iron
Property Overview
Density7.4g/cm³
Elastic ModulusUnknown
Tensile Strength370MPa
Yield Strength210MPa
Brinell HardnessUnknown
Maximum Service TemperatureUnknown
Chemical Composition
Mechanical
A - Min. elongation at fracture (%)
7
KV - Impact energy (J)
+20° 13
R p0.2 0.2% proof strength (MPa)
210
Rm - Tensile strength (MPa)
370
Registered Designations & Aliases
EN-GJSA-XNiCrNb20-2EN-JS3031
Standards
EN 13835 EN 13835: 2002 Founding. Austenitic cast irons