EN-GJS-600-10
Cast Iron
Property Overview
Density7g/cm³
Elastic ModulusUnknown
Tensile StrengthUnknown
Yield Strength470MPa
Brinell Hardness190 - 230HB
Maximum Service TemperatureUnknown
Chemical Composition
Mechanical
A - Min. elongation at fracture (%)
10
A - Min. elongation at fracture (%)
8
R p0.2 0.2% proof strength (MPa)
470
R p0.2 0.2% proof strength (MPa)
450
Hardness
Brinell hardness (HBW):
190 - 230
Other
Nominal thickness (mm):
to 30
Nominal thickness (mm):
30 - 60
Registered Designations & Aliases
5.3110EN-GJS-600-10
Standards
EN 1563 EN 1563: 2011 Founding. Spheroidal graphite cast irons