NiCr22Fe18Mo(dubl)
Nickel Alloys
Property Overview
Density8.3g/cm³
Elastic ModulusUnknown
Tensile Strength690MPa
Yield Strength270MPa
Brinell HardnessUnknown
Maximum Service TemperatureUnknown
Chemical Composition
Mechanical
A - Min. elongation at fracture (%) (+AT)
30
R p0.2 0.2% proof strength (MPa) (+AT)
270
R p0.2 0.2% proof strength (MPa) (+AT)
270
+AT
Rm - Tensile strength (MPa) (+AT)
690
Hardness
+A Soft annealed +AC Annealed to achieve spheroidization of the carbides +AR As rolled +AT Solution annealed +C Cold drawn / hard +CR Cold rolled +FP Treated to ferrite-pearlite structure and hardness range +I Isothermal annealing +LC Cold drawn / soft +M Thermo mechanical rolling +N Normalized +NT Normalized and tempered
+P Precipitation hardened +PE Peeled +QA Air quenched and tempered +QL Liquid quenched and tempered +QT Quenched and tempered +S Treated to improve shearability +SH As rolled and turned +SR Cold drawn and stress relieved +T Tempered +TH Treated to hardness range +WW Warm worked +U Untreated
Registered Designations & Aliases
2.4665NiCr22Fe18Mo(dubl)
Standards
EN 10302 EN 10302: 2008 Creep resisting steels, nickel and cobalt alloys