TS550
Carbon & Non-Alloy Steels
Property Overview
Density-g/cm³
Elastic ModulusUnknown
Tensile Strength575MPa
Yield Strength550MPa
Brinell HardnessUnknown
Maximum Service TemperatureUnknown
Chemical Composition
Mechanical
R p0.2 0.2% proof strength (MPa)
550
Rm - Tensile strength (MPa)
575
Registered Designations & Aliases
1.0385TS550
Standards
EN 10202 EN 10202: 2001 Cold reduced tinmill products. Electrolytic tinplate and electrolytic chromium/chromium oxide coated steel